Material · injection molding

LCP injection molding design guidelines

LCP flows into extremely thin walls and is used for fine-pitch connectors. It shrinks very little along the flow and more across it, so the direction a part fills in decides how it warps. The figures here are for a glass-filled grade.

This page gives the wall thickness PartCheck checks LCP against, the rib, boss and corner sizes that follow from it, and the published processing figures. You can then check your own part, free and in your browser.

LCP wall thickness

A LCP part is checked against a nominal wall of 0.76 mm to 3.05 mm. Thinner, and the plastic may not fill the cavity or will be weak; thicker, and sink marks, voids and cooling time all climb.

LCP is a liquid-crystal polymer: it shrinks little, but unevenly, so PartCheck holds it to the tighter band of the semi-crystalline resins. PartCheck flags regions more than 15% off the part's nominal wall. Where the wall has to change, step it gradually; published guidance keeps neighbouring sections within about 3:1.

Ribs, bosses, corners and draft

These follow from the nominal wall rather than from the plastic, so here they are at the thinnest, middle and thickest wall in LCP's range.

Feature sizes for LCP at three nominal walls
Nominal wall0.76 mm1.90 mm3.05 mm
Rib ≤ 0.6× wall0.46 mm1.14 mm1.83 mm
Boss wall ≤ 0.8× wall0.61 mm1.52 mm2.44 mm
Inside radius ≥ 0.5× wall0.38 mm0.95 mm1.52 mm
Thick section from 2.0× wall1.52 mm3.81 mm6.10 mm
The defaults PartCheck checks against. Every one can be changed to match your molder.
Ribs

A rib thicker than this at its root shows as a sink line on the face behind it. Make it taller for stiffness, not thicker.

Bosses

A screw boss with a thicker wall shrinks harder than the wall it stands on and pulls a sink through to the face opposite.

Inside corners

A sharp inside corner concentrates stress and makes the plastic turn too hard as it flows. Half the wall is the usual radius.

Draft

At least 1° on faces along the direction the mold opens, so the part releases without dragging. Textured faces need more, roughly a degree for every 0.025 mm of texture depth.

LCP processing figures

Published figures for LCP
FigureValue
Grade the figures are forLCP, 30% glass
Density1.61 g/cm³
PartCheck has no published thermal data or cavity pressure for LCP, so it leaves the estimates that need them blank rather than guess.

Check a part in LCP

Open your STEP file in PartCheck's DFM tab, choose injection molding and LCP, and every wall, rib, boss, corner and draft above is checked on your part, with each problem marked where it is. The full list of checks is in the injection molding DFM guide.

Questions

What is the minimum wall thickness for LCP?

0.76 mm is the thinnest nominal wall PartCheck checks LCP against. Thinner sections risk not filling and are weak.

What is the maximum wall thickness for LCP?

3.05 mm. Above it, sinks, voids and cycle time climb; core the section out instead.

How thick should a rib be in LCP?

At most 0.6× the wall it stands on: 1.14 mm on a 1.90 mm wall.

What draft angle does LCP need?

1° is PartCheck's default for every plastic, and more on textured faces.

Try it on a real part

The demo is a moulded enclosure lid in two revisions, drawn in CAD. It opens in the tool with no files needed, or you can open your own STEP files. Nothing is uploaded: the analysis runs in your browser.