PPS is a high-temperature, chemically resistant resin that is almost always molded glass filled, which is why the figures here are for a filled grade. It flows into very thin walls.

This page gives the wall thickness PartCheck checks PPS against, the rib, boss and corner sizes that follow from it, and the published processing figures. You can then check your own part, free and in your browser.

PPS wall thickness

A PPS part is checked against a nominal wall of 0.51 mm to 4.57 mm. Thinner, and the plastic may not fill the cavity or will be weak; thicker, and sink marks, voids and cooling time all climb.

PPS is semi-crystalline. Semi-crystalline resins shrink more, and unevenly, so a wall that varies warps the part. PartCheck flags regions more than 15% off the part's nominal wall. Where the wall has to change, step it gradually; published guidance keeps neighbouring sections within about 3:1.

Ribs, bosses, corners and draft

These follow from the nominal wall rather than from the plastic, so here they are at the thinnest, middle and thickest wall in PPS's range.

Feature sizes for PPS at three nominal walls
Nominal wall0.51 mm2.54 mm4.57 mm
Rib ≤ 0.6× wall0.31 mm1.52 mm2.74 mm
Boss wall ≤ 0.8× wall0.41 mm2.03 mm3.66 mm
Inside radius ≥ 0.5× wall0.26 mm1.27 mm2.29 mm
Thick section from 2.0× wall1.02 mm5.08 mm9.14 mm
The defaults PartCheck checks against. Every one can be changed to match your molder.
Ribs

A rib thicker than this at its root shows as a sink line on the face behind it. Make it taller for stiffness, not thicker.

Bosses

A screw boss with a thicker wall shrinks harder than the wall it stands on and pulls a sink through to the face opposite.

Inside corners

A sharp inside corner concentrates stress and makes the plastic turn too hard as it flows. Half the wall is the usual radius.

Draft

At least 1° on faces along the direction the mold opens, so the part releases without dragging. Textured faces need more, roughly a degree for every 0.025 mm of texture depth.

PPS processing figures

Published figures for PPS
FigureValue
Grade the figures are forPPS, 40% glass
Density1.65 g/cm³
Mean cavity pressure40 MPa
Cavity pressure from Polymer School; it sizes the clamp force a press needs. PartCheck has no published thermal data for PPS, so it leaves the estimates that need it blank rather than guess.

Check a part in PPS

Open your STEP file in PartCheck's DFM tab, choose injection molding and PPS, and every wall, rib, boss, corner and draft above is checked on your part, with each problem marked where it is. The full list of checks is in the injection molding DFM guide.

Questions

What is the minimum wall thickness for PPS?

0.51 mm is the thinnest nominal wall PartCheck checks PPS against. Thinner sections risk not filling and are weak.

What is the maximum wall thickness for PPS?

4.57 mm. Above it, sinks, voids and cycle time climb; core the section out instead.

How thick should a rib be in PPS?

At most 0.6× the wall it stands on: 1.52 mm on a 2.54 mm wall.

What draft angle does PPS need?

1° is PartCheck's default for every plastic, and more on textured faces.

Is PPS amorphous or semi-crystalline?

Semi-crystalline, which is why its walls are held within 15% of nominal.